A cold rolled stainless sheet leaves the mill with two edges that were never cut. That is a mill edge: the width is whatever the rolling mill produces, normally 1000, 1219 or 1500 mm, the edge has a slight crown and a rolled radius, and the strip can wander by a few millimetres over a coil length. Mill edge is cheaper because nothing has to be set up, and it is perfectly adequate when the edge will be trimmed, hidden in a fold, or welded into a seam.
A slit edge has been cut. The coil is uncoiled, passed through rotary knives and rewound to a width the customer specifies. The edge is straight, the width is held to a tolerance, and there is a burr on one face. That is a strip, and the difference matters as soon as the material is fed into a machine: a roll former, a tube mill, a press line or a laser with a fixed sheet size.
So the first question on an enquiry is not the grade or the finish, it is whether the edge will be cut. A mill edge sheet sold as a strip will run off centre in a roll former and jam the line, and no amount of gauge accuracy will fix it.
Three numbers define a slitting job. The width tolerance is normally plus or minus 0.1 mm on widths below 300 mm and plus or minus 0.2 mm above that; a precision line can hold 0.05 mm on narrow strip at a higher cost and a slower pass.
Camber is the straight line deviation over a length. Standard is 1 mm over 2 metres, and a good slitter holds half that. Camber comes from a width variation in the master coil or from unequal tension across the slitter, and it is the defect that ruins long feed runs because the strip steers.
Burr direction is the one buyers forget. Slitting produces a burr on one face, and whether that burr faces up or down in the stack decides whether it marks the mating sheet, whether it catches in a guide, and which way the coil must be unwound. If the part is visible, ask for the burr on the hidden face; if it will be coated or painted, ask for a deburred edge, which is a second pass and costs extra.
| Parameter | Value |
|---|---|
| Grade | 201, 304, 304L, 316L, 430, 409L, 441 |
| Thickness | 0.3 to 3.0 mm cold rolled |
| Width | Mill edge 1000 / 1219 / 1500 mm, slit 20 to 1500 mm |
| Width tolerance | plus or minus 0.1 mm below 300 mm, 0.2 mm above |
| Edge | Mill edge, slit edge, deburred on request |
| Finish | 2B, BA, HL, No.4, 8K, or PVC coated |
| Camber | 1 mm per 2 m standard, 0.5 mm on request |
| Coil | ID 508 or 610 mm, 3 to 15 tonnes |
| Standard | ASTM A240, A480, EN 10088-2 |
| Test | EN 10204 3.1, PMI, thickness report |
Cut to length is available from the same coil, which is normally cheaper than buying a sheet and cutting it yourself once the quantity passes a few tonnes. The cut length tolerance is plus or minus 1 mm on a stop and cut line, and squareness within 1 mm per metre.
201 is the manganese bearing austenitic. It is cheaper than 304 because nickel is partly replaced with manganese, it forms and welds reasonably, and it is suitable for dry indoor work: appliance panels, kitchen cabinet liners, elevator trim, shelving. It stains in a wet chloride environment and it is not a substitute for 304 outdoors.
304 is the default for anything exposed, welded or food related. 316L is the answer where chloride is present: coastal, marine, chemical, swimming pool, and food plants using hypochlorite sanitisers.
430 is ferritic and magnetic, used for appliance and automotive trim where a magnet is not a problem and cost matters. It is less weldable than 304 and its ductility at the bend is lower, so tight folds need a larger radius.
2B is cold rolled, annealed and pickled, then skin passed. It is the standard finish: a slightly grey, matte surface with a low Ra, suitable for painting, forming and most industrial work.
BA is bright annealed, processed in a controlled atmosphere so the surface stays reflective without pickling. It is smoother, brighter and more uniform, and it costs more because the annealing line is slower and the coil must be clean before it enters. A BA sheet that is subsequently bent will show the bend line, and a BA surface that is handled without gloves shows every fingerprint.
HL is a hairline, No.4 is a coarser brushed grain, and 8K is a mirror polish. All three are applied after rolling, and all three are directional. On a visible panel, specify the grain direction on the drawing, because it cannot be changed after cutting.
Can you slit to 43 mm?
Yes, from 20 mm upward on a standard line, with 0.1 mm width tolerance.
What is the minimum quantity for a slit width?
Usually one coil, or a few tonnes. Below that the slitting set up dominates the price.
Do you supply cut sheets as well as coil?
Yes, cut to length with a stop and cut line, packed on a wooden pallet.
Is 201 acceptable outdoors?
No. It will stain within a season in a wet or coastal location. Use 304 or 316L.